Researchers have developed a dual-layer synchronous focused induction heating process for soft soldering through-hole (THT) solder joints on thick printed circuit boards, directly tackling two persistent defects in thick-plate interconnection: insufficient solder penetration rate and excessive void ratio.
The study explored soldering processes for 3 mm, 4 mm, and 5 mm thick plates using a dual-layer synchronous focused induction heating device. The team systematically analyzed how soldering time, heating power, and plate thickness affect solder joint morphology and penetration rate, and determined the optimal process window for each thickness.
Results showed that solder joints produced with the optimal process had complete, defect-free morphology, with no burnt or overheated areas on the printed circuit boards. The pull-out strength of the through-hole solder joints exceeded the tensile strength of the pin material itself, and all joints maintained electrical continuity. Most notably, the solder penetration rate reached 100% across all thick-plate through-hole joints.
Microstructural analysis via scanning electron microscopy (SEM) and energy dispersive X-ray spectrometry (EDX) revealed that solder wetted and spread along both sides of the pads, forming a characteristic skirt-shaped joint structure at the upper and lower pads. A dense intermetallic compound (IMC) layer formed at the interface between the Cu pads and SAC305 solder, with IMC thickness measuring between 1 and 3 μm — an indicator of a sound metallurgical bond.
Reliability was validated through temperature cycling tests. After 500 thermal cycles, the solder joint surfaces remained bright with no cracks, pinholes, or desoldering. Pull-out testing again showed pin fracture while the solder joints remained intact; all circuits stayed conductive and the solder penetration rate held at 100%.
The authors conclude that dual-layer synchronous focused induction heating soldering can reliably achieve through-hole solder joint interconnection on thick plates of varying thicknesses, delivering good mechanical properties and long-term reliability. The process offers an effective industrial solution for thick-plate through-hole interconnection challenges commonly encountered in power electronics, industrial control, and high-reliability electronic assembly.