Researchers publishing in the Chinese journal Welding (Harbin Welding Institute) have demonstrated that a dual-layer synchronous focused induction heating approach can produce reliable through-hole solder joints on thick printed circuit boards, tackling two chronic defects in this interconnection method: insufficient solder penetration and void formation.
The challenge
Through-hole insertion (THT) soldering on thick boards is widely used where high mechanical strength and current-carrying capacity are required, but as board thickness grows, molten solder struggles to fill the barrel completely. Incomplete penetration and voids undermine both electrical continuity and joint strength. Conventional reflow and iron-based methods become increasingly difficult to control as plate thickness increases.
The method
The team used a dual-layer synchronous focused induction heating device to explore soldering processes for through-hole joints on 3 mm, 4 mm, and 5 mm thick plates. They systematically analyzed how soldering time, heating power, and plate thickness influence joint morphology and solder penetration rate, and from these experiments established the optimal process window for each thickness.
Results
Joints produced with the optimized process showed complete, defect-free morphology — no burnt or overheated damage was observed on the printed circuit boards. Key findings:
- Strength: pull-out strength of the through-hole joints exceeded the strength of the pin material itself, so mechanical failure occurred in the pin rather than the joint.
- Penetration: solder penetration rate reached 100% on thick-plate through-hole joints.
- Interfacial structure: SEM and EDX analysis showed solder wetting and spreading along both pads, forming a characteristic "skirt-shaped" joint at the upper and lower pad surfaces. A dense intermetallic compound (IMC) layer formed at the Cu pad / SAC305 solder interface, with IMC thickness measured between 1 and 3 µm — within the range typically associated with good joint reliability.
- Reliability: after 500 temperature cycles, joint surfaces remained bright with no cracks, pinholes, or de-soldering. Pull-out testing still resulted in pin fracture while the solder joints remained intact, all circuits stayed conductive, and the 100% penetration rate was maintained.
Conclusion
The study concludes that dual-layer synchronous focused induction heating soft soldering can reliably achieve through-hole joint interconnection across different thick-plate configurations, delivering good mechanical performance and long-term reliability. The work offers a practical solution for thick-plate through-hole interconnection in electronics manufacturing, where board-level assembly quality directly affects the durability of industrial, automotive, and power electronics.